Welcome to Vbond

When buyers compare aluminum composite panels (ACP), they often see terms such as "70% PVDF," "high-performance PVDF," and "standard PE coating." These labels sound simple, but they do not tell the whole story.
The most important question is what the 70% figure actually measures. Does it mean 70% of the liquid paint? Does it refer to the resin blend? Or does it describe only the color coat?
In many architectural coating specifications, 70% PVDF means that PVDF resin makes up at least 70% by weight of the total resin content in the color coat. The remaining resin is often acrylic. It does not normally mean that 70% of the entire liquid paint consists of PVDF.
This distinction matters when purchasing a PVDF Alucobond panel. A buyer needs to understand the coating formula, the measurement basis, and the supporting documents before accepting a supplier's claim.
This guide explains what resin content means, how PVDF and PE coatings differ, and how to verify a 70% PVDF specification.
A coating contains more than one ingredient. Resin is only one part of the formula, but it plays a central role in forming the protective film.
A typical liquid architectural coating may contain:
· Resin: Forms the film and binds the coating ingredients together.
· Pigments: Provide color, opacity, and certain performance properties.
· Solvents: Control flow and application. Most of the solvent leaves during drying or curing.
· Additives: Adjust flow, surface appearance, curing, and other properties.
Resin affects how the coating performs after application. It influences weather resistance, flexibility, adhesion, surface hardness, and resistance to UV-related degradation.
Pigments and additives also matter. Two coatings with the same resin ratio can perform differently if they use different pigments, additives, or production methods.
Illustration of PVDF coating components, including PVDF resin, acrylic resin, pigments, solvents, and additives.
A typical 70% PVDF architectural coating uses a blend of PVDF and acrylic resins. Pigments, solvents, and additives complete the formula.
Component | Main Function | Effect on the Coating |
PVDF resin | Forms the main fluoropolymer part of the binder | Supports weather and UV resistance |
Acrylic resin | Works with PVDF in the binder system | Supports film formation, adhesion, and other physical properties |
Pigments | Provide color and opacity | Affect color stability and appearance |
Solvents | Control liquid flow and application | Support coating application and film formation |
Additives | Adjust specific coating properties | Affect flow, curing, and surface quality |
The exact formula varies by coating manufacturer and product series. Buyers should request the technical data for the actual coating used on the panel.
The 70% figure usually describes the share of PVDF resin within the coating's total resin blend.
For example, imagine a color-coat binder that contains 100 kg of resin solids:
Resin Component | Weight | Share of Total Resin |
PVDF resin | 70 kg | 70% |
Acrylic resin | 30 kg | 30% |
Total resin | 100 kg | 100% |
In this example, PVDF makes up 70% of the resin blend. Acrylic makes up the other 30%.
The formula may also contain pigments, solvents, and additives. Those ingredients are not included in this simple 70:30 resin calculation.
Consider a liquid coating that contains:
· 40 kg of total resin solids
· 20 kg of pigments and other nonvolatile ingredients
· 40 kg of solvent
If PVDF accounts for 70% of the resin solids, the formula contains 28 kg of PVDF resin.
That means:
· PVDF is 70% of the resin solids.
· PVDF is 28% of the total 100 kg liquid coating.
The example shows why buyers must ask for the calculation basis. A statement such as "70% PVDF" is incomplete unless the supplier identifies what the percentage refers to.
Some coating systems also use a minimum PVDF share of total coating solids as a separate requirement. This is not the same calculation as the PVDF share of total resin.
Measurement Basis | What It Measures | What Buyers Should Confirm |
PVDF as a percentage of total resin | PVDF weight divided by total resin weight | Is the resin blend at least 70% PVDF? |
PVDF as a percentage of total coating solids | PVDF weight divided by all nonvolatile coating ingredients | What is the minimum PVDF share of total solids? |
PVDF as a percentage of wet paint | PVDF weight divided by the full liquid coating weight | Is this figure being used correctly and clearly? |
Procurement rule: Never compare two PVDF percentages until both suppliers confirm the same measurement basis.
PVDF provides strong weather resistance, but a coating needs more than one property to perform well.
Coating manufacturers often blend PVDF with acrylic resin to balance weatherability with film formation, adhesion, hardness, and flexibility. The acrylic component supports the coating system while the PVDF component provides much of its long-term weather resistance.
A 70:30 PVDF-to-acrylic resin ratio is widely used in high-performance architectural coating systems. Some established coating systems also set additional requirements for PVDF content as a percentage of total coating solids.
The ratio is not a guarantee of performance by itself. The quality of the raw materials, pigment selection, pretreatment, application, and curing process also affect the finished film.
Coating System | Resin Composition | General Characteristics |
Standard PE | Polyester-based resin system | Commonly used for decorative and selected interior or exterior applications |
PVDF/acrylic blend | Often specified at 70:30 by resin weight | Combines PVDF weather resistance with acrylic film properties |
Other PVDF blends | Depends on the coating manufacturer's formula | Must be assessed using the actual technical specification |
Do not assume that every coating with a PVDF label uses a 70:30 resin blend. Likewise, do not assume that every PE coating uses the same polyester formula.
Ask the supplier to identify the coating manufacturer, product series, resin system, and applicable performance specification.
PE and PVDF coatings use different resin systems. This difference affects how the coating responds to long-term outdoor exposure.
Standard PE coatings commonly use polyester resin. They offer good decorative performance and can suit applications where the project does not require the weathering performance of a high-performance fluoropolymer coating.
A 70% PVDF coating uses a resin blend in which PVDF forms the majority of the binder. It generally provides better resistance to UV-related degradation, color change, and chalking when properly formulated and applied.
Item | Standard PE Coating | 70% PVDF Coating |
Main resin system | Polyester | PVDF and usually acrylic |
Typical resin blend | Varies by product | Often 70:30 PVDF/acrylic |
UV resistance | Generally lower | Generally higher |
Color retention | More limited under demanding exposure | Generally stronger |
Chalking resistance | Depends on formulation | Generally stronger |
Outdoor use | Selected exterior applications | High-performance architectural applications |
Initial cost | Usually lower | Usually higher |
Main buying concern | Confirm the product's intended exposure | Verify resin content and coating performance |
These are general differences, not a substitute for test results. A poorly made PVDF coating may underperform a well-made alternative coating system.
Buyers should compare actual coating data rather than judge a panel by the PE or PVDF label alone.
No. Resin content is an important specification, but it does not measure every part of coating quality.
A coating can meet a 70% PVDF resin ratio and still perform poorly if the manufacturer uses unsuitable pigments, poor pretreatment, or an incorrect curing process.
A reliable PVDF Alucobond panel needs a complete and controlled coating system.
1. Resin quality
The coating manufacturer should identify the PVDF resin system and provide supporting product information. Buyers should not rely on a generic statement that the coating contains "premium PVDF."
2. Pigment quality
Pigments affect color, opacity, and weathering behavior. Some colors and metallic finishes require special pigment systems, so the same resin ratio does not guarantee identical results across all colors.
3. Aluminum pretreatment
The coating needs a clean, properly treated aluminum surface. Poor surface preparation can weaken adhesion and increase the risk of coating failure.
4. Film thickness
The dry film thickness (DFT) must meet the specified coating system. A coating with the correct resin ratio can still fail to meet the project requirement if the applied film is too thin or uneven.
5. Curing and production control
The coating manufacturer must follow the correct application and curing conditions. Poor curing can affect film formation, adhesion, and final coating properties.
"Diagram showing PVDF resin content, pigment quality, aluminum pretreatment, dry film thickness, and curing as factors in ACP coating quality"
A professional buyer should evaluate all five factors together. The resin percentage confirms one part of the formula, not the quality of the complete panel.
No. The percentage normally refers to a specified coating layer, not the entire aluminum composite panel.
An ACP panel contains aluminum skins, a core, and coating layers on its surfaces. The exposed color coat is usually the main focus when a specification calls for a minimum PVDF resin content.
The primer and back coating may use different formulations. A three-coat system may also include a clear coat with its own resin-content requirement.
Layer | Main Purpose | What Buyers Should Check |
Clear coat, if used | Adds a surface layer and supports the specified finish | Resin system and whether the 70% requirement applies |
Color coat | Provides the visible color and main decorative finish | PVDF resin percentage and DFT |
Primer | Supports adhesion and corrosion protection | Primer type, thickness, and compatibility |
Pretreatment | Prepares the aluminum surface | Process and quality control |
Aluminum skin | Provides the metal face of the panel | Alloy, temper, and thickness |
Core | Connects the two aluminum skins | Core type and required fire performance |
For example, a specification may require a minimum of 70% PVDF resin by weight in the color coat. That wording does not automatically mean the primer, back coating, and clear coat all meet the same ratio.
Buyers should state the required coating layer in the purchase specification. This avoids disputes when the supplier and customer use different definitions.
A product brochure may state "70% PVDF," but a professional purchase should rely on traceable documents.
Ask the supplier to provide evidence from the coating manufacturer. The documents should identify the coating product, resin system, and measurement basis.
Document | Information to Check |
Coating Technical Data Sheet (TDS) | Product name, coating type, recommended application, and film thickness |
Resin manufacturer's statement | PVDF resin identity and applicable resin-content requirement |
Coating formulation declaration | Whether the 70% figure refers to total resin or another basis |
Coating manufacturer's certification | Confirmation of the specified coating system |
Quality inspection report | Actual coating thickness, appearance, and relevant test results |
Batch or production record | Traceability between the coating product and supplied panels |
A panel supplier may purchase coated aluminum coil from another manufacturer. In that case, ask for documents that link the coating specification to the actual coil and production batch.
A general brochure is useful for initial screening. It is not enough to prove that a specific order meets the project requirement.
1. Who manufactures the coating?
2. What is the exact coating product name and series?
3. Does 70% refer to PVDF by weight of total resin solids?
4. Does the requirement apply to the color coat, clear coat, or both?
5. What is the specified dry film thickness?
6. Can the supplier provide a coating manufacturer's declaration?
7. Can the supplier trace the coating batch to the delivered ACP panels?
Clear answers make supplier comparison more reliable and reduce the risk of buying a product that does not match the specification.
Buyers often see "70% PVDF" and "AAMA 2605" listed together. These terms describe different parts of the coating specification.
The 70% figure describes resin composition under a stated calculation basis. AAMA 2605 is a performance specification for high-performance organic coatings on architectural aluminum extrusions and panels.
A project specification may require both a minimum PVDF resin percentage and compliance with AAMA 2605. Buyers should not treat one as automatic proof of the other.
Requirement | What It Tells You | What It Does Not Prove by Itself |
70% PVDF resin content | The specified PVDF share of the resin blend | Full coating performance |
Dry film thickness | The thickness of the cured coating film | Resin composition |
AAMA 2605 compliance | Performance against the specified coating requirements | The exact resin percentage unless separately stated |
Adhesion test | How well the coating adheres under the test conditions | Long-term outdoor performance by itself |
Weathering test | How the coating responds under defined exposure conditions | A guaranteed number of outdoor service years |
When a project requires AAMA 2605, ask for documentation that identifies the specific coating system and confirms that the relevant product meets the required specification.
Also check whether the document covers the actual color, finish, primer, and clear coat used in the order. Do not assume that a certificate for one coating system automatically covers every product in the supplier's range.
Imagine a contractor is sourcing 4,000 square meters of PVDF aluminum composite panels for a commercial facade.
Two suppliers submit quotations:
Item | Supplier A | Supplier B |
Coating description | 70% PVDF | Premium PVDF |
Resin-content basis | 70% of total resin | Not stated |
Coating manufacturer | Identified | Not identified |
Color-coat thickness | Declared | Declared, but no test record |
AAMA 2605 documentation | Available | Not provided |
Batch traceability | Available | Not confirmed |
Supplier B may offer a lower price, but its description does not provide enough information to verify the coating.
The contractor should request the missing documents before comparing the two quotations. If Supplier B cannot confirm the resin-content basis or provide relevant coating evidence, the contractor cannot treat the two products as technically equal.
· Confirm the exact PVDF resin-content definition.
· Request the coating manufacturer's product data.
· Verify the color-coat dry film thickness.
· Check the required performance standard.
· Confirm the production batch and coating source.
· Compare prices only after both products meet the same specification.
The lowest quotation should not win simply because it uses the word "PVDF." A clear technical specification protects the buyer from hidden differences.
Vague wording creates room for different interpretations. A strong purchase specification defines the resin percentage, the coating layer, the film thickness, and the required performance.
The following is a sample clause. Buyers should adjust it to match the project's approved design and coating system.
Exposed aluminum faces shall receive a factory-applied PVDF coating system. The color coat shall contain not less than 70% PVDF resin by weight of the total resin content in the color-coat binder. The supplier shall identify the calculation basis and provide supporting documentation from the coating manufacturer.
The coating system shall meet the project-required performance specification. The supplier shall state the primer and color-coat dry film thickness, identify the coating product, and provide relevant quality and compliance documents.
Any clear coat or back coating shall be identified separately. The supplier shall not apply the 70% PVDF requirement to other coating layers unless the project specification states so.
This wording makes the measurement basis clear. It also prevents a supplier from using a general PVDF label as a substitute for product evidence.
Supplier claims 70% PVDF
|
Identify the coating product
|
Confirm the percentage basis
|
Check which coating layer it covers
|
Review resin and coating documents
|
Verify DFT and required performance
|
Approve the coating specification
|
Confirm production batch traceability
This process gives procurement teams a repeatable way to review coating claims before placing an order.
This is usually incorrect. In common architectural coating specifications, the figure refers to the PVDF share of the total resin content in the specified coating layer.
Not necessarily. Resin quality, pigment selection, pretreatment, film thickness, and curing all affect the final result.
It does not. Resin composition and coating performance are separate requirements. Request the relevant compliance documents.
Not automatically. A specification may apply the requirement only to the color coat. Check the wording for primer and clear-coat requirements.
Different coating manufacturers use different formulations and product systems. Confirm the exact product rather than relying on a generic label.
The phrase "70% PVDF" has a specific technical meaning in many architectural coating specifications. It commonly refers to PVDF resin making up at least 70% by weight of the total resin content in the color coat, rather than 70% of the complete liquid paint.
For buyers comparing a PVDF Alucobond panel with a standard PE-coated ACP panel, this distinction is essential. It helps separate a documented high-performance coating system from a product that carries only a general marketing claim.
However, resin content is only one part of coating quality. Buyers should also verify the coating manufacturer, product series, pigment system, pretreatment, dry film thickness, curing process, and required performance documents.
A reliable purchasing decision starts with a clear question: 70% of what, in which coating layer, and supported by which document?